Solution
Non-contact crack detection without sensors on the component
A crack changes how a component vibrates. Non-contact vibration analysis measures this change point by point across the entire surface, without bonded sensors, cables or added mass. It can reveal subsurface damage that a camera cannot see and that may go undetected between individual sensors.
6 min read


Waves travelling through a carbon fibre plate reveal hidden defects. Research teams have tested the method on wind turbine blades, fibre-reinforced composite plates and metal parts, using a laser Doppler vibrometer to measure the vibrations.
Where conventional crack detection methods reach their limits
The aim is to detect cracks and delaminations before they weaken a component. Many established inspection methods cover only part of the component or influence the response being measured.
Cameras and drones see only the surface
Optical imaging detects cracks that are visible on the inspected surface. Damage inside the component or on the reverse side remains hidden.
Bonded sensors change the vibration response
An accelerometer adds mass. On lightweight or thin-walled components, that extra mass alters the very vibration the sensor is intended to measure.
Sparse measurement points leave gaps
Fixed sensors take measurements only where they are mounted. Damage between sensors can easily go undetected.
Non-contact vibration analysis addresses all three limitations. It scans the surface point by point without contact or added mass, taking measurements at thousands of locations if needed.
How non-contact crack detection works
A crack reduces local stiffness and changes the vibration response. The crack scatters waves, and the frequencies at which the component vibrates most strongly shift. These changes can be measured at the surface even when the damage is internal or on the reverse side.
- 1. Excite the component
- A single tap with an impulse hammer is enough. A shaker or a small piezoelectric element attached to the component provides repeatable excitation.
- 2. Scan the surface
- At each point on a grid, a laser beam measures the velocity of the surface without a sensor attached at the measurement point.
- 3. Identify anomalies
- An animation shows how vibration propagates through the component. The frequency spectrum reveals departures from the expected vibration response.
- 4. Assess the findings
- Comparison with an undamaged component helps interpret any deviations. For routine inspections, the quantities to measure and their acceptance limits can be defined in advance.
What studies have shown
Estimating crack length
Researchers used waves scattered by a fatigue crack in an aluminium plate to estimate its length at 31 millimetres. The actual crack length was 30 millimetres.
Distinguishing cracked parts from intact parts
In tests on gears made from compacted steel powder, the resonance peaks shifted or split in the two damaged gears.
Locating hidden damage
At certain frequencies, two regions of a carbon fibre-reinforced polymer (CFRP) plate vibrate more strongly than the surrounding material. Measurements taken from the front reveal the locations of defects on the reverse side.
Comparing crack detection methods: ultrasonic, liquid penetrant, magnetic particle and eddy current testing
Each method has its strengths. Non-contact vibration analysis complements conventional inspections where contact, inspection media or added mass are inadmissible, or where the aim is to assess the component as a whole.
| What the inspection reveals | What the inspection requires | |
|---|---|---|
| Non-contact vibration analysis | Where and how the component vibrates. Changes in wave propagation or resonance can indicate cracks, including those below the surface. | An excitation source and a clear line of sight to the measurement surface. Measurements are taken from a distance. |
| Visual inspection using a camera or drone | Cracks visible at the surface | A clear line of sight and adequate lighting |
| Ultrasonic testing | Echoes from surface and internal flaws | A couplant to transmit sound when using conventional contact probes |
| Liquid penetrant testing | Fine surface-breaking cracks | A clean, largely non-porous surface and a liquid penetrant |
| Magnetic particle testing | Surface and near-surface flaws | A ferromagnetic material |
| Eddy current testing | Small surface and near-surface cracks | An electrically conductive material and access for the probe |
Case study: detecting cracks in a wind turbine blade
Wind turbine blades are large composite structures that are difficult to access. In 2024, a research team investigated whether non-contact measurements could detect cracks in a 45-centimetre prototype blade made of glass fibre-reinforced polymer (GFRP). The team compared three blade conditions: intact, with a shallow crack and with a deep crack.
Measurement on the prototype rotor blade. Image: Zabihi et al. 2024, CC BY 4.0
Measuring on either side of the damage
A small piezoelectric element on the blade generated short wave pulses. A single-point laser Doppler vibrometer from the Nova series, now called CLASSIC Nova, measured surface motion on either side of the damaged area. Reflective tape was applied at the measurement points.
The team recorded the signals using OptoGUI. The researchers then compared the frequencies present in the signals from the intact and damaged blade.
The deep crack produces an additional frequency component
The middle row of plots below shows the frequency components for all three blade conditions. The axis scales vary between plots.
- On the excitation side of the damage, the blade with the deep crack showed a distinct additional frequency component at around 400 kilohertz (kHz). This component was absent in the intact blade.
- Beyond the damaged area, both cracks produced a broader spread of vibration frequencies around the excitation frequency of 200 kHz.
Is this method suitable for your component?
For an initial assessment, provide the material, component dimensions and suspected crack location. These details help determine which side to measure from and which excitation method suits the inspection.
Applications of non-contact crack detection

Hidden damage in fibre-reinforced composites
Defects on the reverse side of CFRP plates show up in the wavefield. Researchers have also used mode shapes to locate crack-like flaws machined into hollow composite beams.

Final inspection of turbine blades
Each blade vibrates most strongly at particular frequencies. Final inspection can verify that these natural frequencies fall within the approved limits.

Loose rivets in aircraft
A loose riveted joint changes the local vibration pattern. The change shows up in the scan even when the joint is difficult to see from the outside.
Using vibration data for automated crack detection with AI
The measurements provide time histories and frequency spectra that can serve as training data for an AI model. The measurement systems do not include a pre-trained model. Users develop the model in their own analysis environment.
Export measurement data
- SMART Lab provides time histories and frequency spectra for further analysis.
- Exported data can be processed further in tools such as MATLAB.
Train your own model
- Measurements from intact and damaged components serve as training examples.
- Train the model in your own analysis environment and test it there on additional components.
Researchers tested this approach on concrete using an impulse hammer and a laser Doppler vibrometer. A neural network analysed the frequency spectra and detected flaws. In a separate study of bonded joints in wind turbine blades, a model initially learned from simulations. Measurements on actual blades improved its predictions. The authors identify collecting field data as the next step towards use on turbines in service.
Measurement systems for non-contact crack detection
The SMART Scan+ scans the surface point by point, measuring vibration velocity at each location. SMART Lab combines the measurements into an animation that shows the path of each wave.
The vibrometer has a built-in signal generator for excitation. It can reproduce the same excitation as often as needed, for example to compare two components directly. The SMART 3D-Scan also captures in-plane motion, measuring all three spatial components of vibration simultaneously.
Frequently asked questions about non-contact crack detection
Can the method detect cracks without sensors on the component?+
Yes. The measurement point requires neither a sensor nor a cable. The component still needs to be excited, for example with an impulse hammer, a shaker or a small piezoelectric element.
Is access to the reverse side of the component necessary?+
Not always. In a test on a carbon fibre plate, measurements from the front were sufficient. Defects on the reverse side altered the wavefield at the measured surface.
Can the method determine crack size?+
In an aluminium plate, researchers used scattered waves to estimate the length of a fatigue crack to within one millimetre. The smallest crack size that can be resolved depends on the component and the analysis method.
Is the method suitable for production testing?+
A few predefined measurement points are often sufficient for comparing turbine blades. The same positions can be used for each blade, and the measured parameters can be checked against approved limits.
Can AI automate crack detection?+
Measurement data can be exported and used to train a custom AI model. Studies on concrete and wind turbine blade joints demonstrate this approach. Model training and testing take place in your own analysis environment.
Sources on measurements and inspection methods
Experimental studies on components
- Zabihi, A., Aghdasi, F., Ellouzi, C., Singh, N. K., Jha, R. and Shen, C. (2024). Non-Contact Wind Turbine Blade Crack Detection Using Laser Doppler Vibrometers. Energies 17, 2165.
- Xiao, W., Yu, L., Joseph, R. and Giurgiutiu, V. (2020). Fatigue-Crack Detection and Monitoring through the Scattered-Wave Two-Dimensional Cross-Correlation Imaging Method Using Piezoelectric Transducers. Sensors 20, 3035.
- Pacheco-Chérrez, J., Cárdenas, D. and Probst, O. (2021). Experimental Detection and Measurement of Crack-Type Damage Features in Composite Thin-Wall Beams Using Modal Analysis. Sensors 21, 8102.
- Tatarinov, A., Kurtenoks, V. and Mironovs, V. (2021). Detection of cracks in green products of powder metallurgy by means of laser vibrometry. Materials Science and Engineering 1140, 012045.
- Zdziebko, P., Krzemiński, M., Okoń, M., Loi, G., Aymerich, F., Pieczonka, Ł. and Klepka, A. (2023). An Approach to the Automated Characterization of Out-of-Plane and In-Plane Local Defect Resonances. Materials 16, 3084.
The photograph and both measurement plots come from the wind turbine blade study by Zabihi et al. and are licensed under Creative Commons Attribution 4.0.
Studies on AI-based analysis
- Muramatsu, Uchida and Takahashi (2020). Noncontact detection of concrete flaws by neural network classification of laser doppler vibrometer signals. Engineering Research Express 2, 025017.
- Kim, H., Kim, H. and Kang, K. (2024). Accuracy Improvement of Debonding Damage Detection Technology in Composite Blade Joints for 20 kW Class Wind Turbine. Machine Learning and Knowledge Extraction 6, 1857–1870.
Background on the inspection methods
The Center for Nondestructive Evaluation at Iowa State University describes the requirements for ultrasonic testing, liquid penetrant testing, magnetic particle testing and eddy current testing.
Further reading
- Materials research
Locate defects on the reverse side of a composite plate.
- Turbine blade inspection
Compare natural frequencies after manufacture or repair.
- Aerospace
Identify loose riveted joints from their vibration patterns.
- Short-wave infrared laser measurements
Measure vibration on dark and matt surfaces.
- Original wind turbine blade study
Measurement setup, plots and results from Zabihi et al.